Default anodize thickness

I recently ano'd a PM7 and was told the manifold for the solenoid is not matching up properly after 200 fps or so ive ano'd a few other matrix's and never had this problem what could have caused this here are my specs roughly as i did this gun a few weeks ago and dont remember exactly.

tank temp 70* very constant
amperage 3.2-3.5 (just the gun body itself)
Length of time in bath 1hour 30 mins.