Yesterday I coated a small bracket with xtreme chrome and it looked great but the flamboyant blue topcoat didn't adhere that well. My question is how am I supposed to get a good ground after the chrome is applied

. I clamped the clip to the chrome but the blue stayed real powdery and came off in spots when I transported to the oven. Thanks for any help!. This site is awesome!