In regards to plating a firearm, I use Brownells blue and rust stripper but about any good stripper will work, you just want to be sure its not too strong. After chemical stripping I polish as required then degrease and clean per the book(Caswells)then plate. I have done many in EL nickle, gold and regular nickle.