Default Re: Vacuum Sand Blaster

I used the shop vac and brush on my blaster today in the chest freezer cabinet.
As I thought, it worked good on areas the brush got a decent seal but around holes or edges it did not work that good, blow by.

For today between rains, I just set up the brush for suction for quick test, not the feed lines yet from the tank.
I have a problem though, Oxide media is giving me nasty headaches! I did not use the cabinet for a few days, I could smell the Oxides when working in it today connecting things up, no blasting yet!
I did not open it after blasting today. I have a nasty headache, I only had these like this a few times and it's since I started blasting and only days I do anything around the blast area.
I do not normally have sinus or other type headache problems, but this is a bad one I get after blasting. I won't be doing much more for blasting for awhile till I fix somethings. Last few headaches I thought was from lack of sleep or lack of food since I had not slept well or eaten much those days. It's about 2-3 hours latter after being around the blaster when I get the headaches and they last all night.
Yes I was wearing a dust filter mask before too.