Default Re: GSXR midpipe High temp gloss black

looks real nice. i'm going to shoot some of this soon, and i have no experience with the high-temp silicone powders. did you follow the cure schedule of 450 for 20min? i remember a thread where someone had trouble with the high-temp cure.