Newbie Here
I have managed to use the Plug and Plate Copy Chrome kit succesfully and will post pictures later. Plating hood and door strikers, I need to add more solution, does this affect the solution that I already have used if I just add more to it? Strikers take alot of abuse, will it peel off as because the plating is so thin?
|