Yes, clean with acetone before powder coating, it removes finger oils etc... for a clean part.
Many recomend wiping with a clean lint free rag and acetone, some say they spray it on from a squirt bottle.
Run a propane torch over the part to burn off any lint from rags etc... and dries it, just a quick pass don't need to heat the part. Keep flames away from acetone and such, propane on the part should be fine, make sure well ventilated when using it and close and remove can before using an open flame in the area. I think acetone is very flamable.