OK,so I went ahead and did them seperately.I taped them all off and used aluminum foil to cover completely. This with blasting and cleaning took nearly two hours to do. I also had to sand down all the sharp edges on the covers.They came out nicer then when I did them assembled in a gig.Sorry I don't have a picture as my buddy already has the rocker covers. With the total amount of time involved I now know why pros charge so much to do these and why Harley only varnishes the rocker covers on their dynas.