first i would not sandblast the chrome off , there are other ways of doing that won t damage the material as much .
blasting chrome off on alumiium could seriously damage some parts .you are trying to blast a very hard material with very abrasive media on a very soft material.
i also think like mpierich said ,(If you have to polish that much after the plating, the part was too rough to begin with.)
|