I do it cold all the time , but remember it takes a long time to reach temp (about 1 hour or more), remember you have to start cure time once the block has reach the temp not the oven ,so don't worry about opening the door it's the only way you will be able to messure the temp.
I use alluminum foil and green tape to mask .
|