If you sandblast a greasy part, you actually POUND the grease INTO the surface.

You should ALWAYS degrease BEFORE sandblasting.

As for naptha etc. These items are really only good at removing OILS, not greases. You need the action of sodium hydroxide (lye) which chemicallly changes the grease into a water miscible soap.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote