Re: What's The Best Way To Repair Plastic Pieces ??
the best way to repair plastic is using 3m duramix products u can find them at auto body supply store. don't waste ur time with the plastic welder too much identification ****. Use the 4040, or the 4058 that stuff sticks to every thing and doesn't crack kind of hard to sand once cured but that's good I guess. Hope that helped
|