Thanks for the reply. I don't think it's a powdercoating. It seems more like a rubbery latex coating. Kinda like dried latex enamel house paint. Once a bit of it flakes off and you pull on it, it stretches. As for the propane, I had actually thought of that. I was worried that I might discolor the aluminumm, though. What do you think?