Re: What am I doing wrong?
I am using a Motorgaurd air filter, and a coiled copper air cooler. I never have used oil in the lines. I figured the phosphate and water wash would take care of any towel dust particles. I have seen a couple feathers here and there, but they are around sharp edges, etc, not in the middle of a flat spot.
I'll use a different can of powder next batch.
I may be only shooting textered powder if this keeps up.
|