View Single Post
  #6 (permalink)  
Old 10-16-2007, 08:55 AM
Harleydad's Avatar
Harleydad Harleydad is offline
Metal Finishing Guru
 
Join Date: Dec 2006
Posts: 733
Harleydad will become famous soon enoughHarleydad will become famous soon enough
Default Re: What am I doing wrong?

After the Acetone blow the part off with clean dry air. After the water rinse blow off with clean dry air and run small propane torch over the part to help remove any rag lint or dust bunnies still remaining. Lint free rags (microfiber) may also help. I think I'm with bandit on the contaminated air.

Last edited by Harleydad; 10-16-2007 at 08:59 AM.