Default Re: On going power supply question??

Quote:
Originally Posted by MrPontiac View Post
.. if the copper pipe is corroded very badly would that cause it
No, that would have the opposite effect.

Voltage would go high, and current would drop low. A complete loss of connection would be an effective open circuit, and current would be zero.

Quote:
I clean the pipe every time i use my rectifier, but after about 15 parts its corroded pretty badly.
I run into the same issue, and clean the pipe as soon as I see visible corrosion.