I built my booth like a closet. 5'w, 5'd, 7't With an exhaust fan in the back of it. Works good. I have a bench piece I slide in to catch the waste powder. It's a piece of 5/8" MDF. Nice and smooth adn powder doesnt stick to it. I use it when I am doing large batches to catch the waste and I reclaim it. get 1 cup reclaim for every 3 cups sprayed. Sometimes I am spraying 7-10 pounds a day, so reclaim adds up fast