I've tried anodizing aluminum foil to see if I could make cheap color chips I can send in the mail. When the ano run was done, there was nothing left.
I have to think that the foil will soon disappear.
If you need some lead sheet, I have some, but shipping will not be cheap. You can find it pretty reasonable at roofing supply stores.