I bought a new 3 gallon copy cad kit, and when I opened up the package, I immediately noticed the "copy cad part B" powder has clumped into very hard lumps, the size of medium pebbles.

I looked in the manual, and online but could not find any specific directions as far as making up the tanks, or if anyone else had this problem before.

So I heated up 3 gallons of water to 115 F and added a few of the "pebbles" to see if they would dissolve in the heated water, but it did not, even after stirring... does it break up after time? any suggestions?