Default Re: what is needed for plating

I bought the wheel Chroming kit I can plate a 20" wheel. Then I had to buy a 35 gal Acid copper, 35 gal chrome stripper, Pickle #4 , and other pickle tanks. I also have built a overhead trolly to hang wheels. Water filter. Dont forget all the sanding and buffing equipment. Let me know if I can help. Thanks, Todd