Quote:
Originally Posted by eshine
But is it better than the Caswell gun? I am not far from purchasing this gun and would love to know. I cant handle the caswell gun, clumpy powder distribution, cup bases seperating from the gun, non-detachable cables make cleaning the gun a bitch.
|
The EW gun will be pretty much the same. Inconsistent powder delivery is just the nature of cup guns. If the powder is clumping out of the caswell gun, you most likely have to much powder in the cup.