Thanks for the replies. That helps me. I told this guy if he wanted to do this I needed some time to get it together with a larger setup. Right now he is giving me some small parts to work with. Let me ask another question?

I have a tank setup with 8 gals of ano solution and a 8 gal rinse tank. I am a newbie at this so please bear with me. I know to clean the part and rinse in Distilled water but do I need to do anything else to ano this part? He just wants it Black with no polishing beforehand. The part is aluminum and about 6 sq inches.