Smile Re: sand blasting cabinet...relocated to tips n tricks section

if you have the time and a wire welder i made me cabinent out of a used wide 2 drawer filing cabinent that i picked up for free, i cut out the bottom and used the metal from the drawers to make the feed for the siphon, i used 2-- 4 inch pvc toilet flanges $8 that screwed into the front and hose clamped the $3 gloves on the inside. used the drawers to make the side door and a $10 piece of plexiglass for the front, cut a hole and bolted a piece of my shopvac hose to the side, i used 2x3's for the frame to set it on--free wood, got a $8 flourescent light from biglots, and a piece of expanded sheetmetal for the floor-- $12, it was cheap, came out good, works good and got to practice my welding at the same time.