I don't know if there are any special requirements. With powder you are attempting to keep the powder from floating out and getting into everything. So with an exhaust fan and filters you can trap most of the powder within the spray area.
Here is a picture of a small powder booth I made.
http://img88.imageshack.us/img88/1488/dcp0908ht7.jpg