i have seen filtration units that are intended for both powder and wet paint. i think it required a filter change. paint filters tend to be much coarser than powder filters. since paint sticks to the filter fibers, the fibers can be pretty loose. and if the fibers were fine like powder filters, they would clog very quickly.