Default Gold Plating multiple items at once

I would like to Gold Plate 30 or more small items at once. The items are small nickel nuts (.5in tall by .25in wide).

I have purchased the Gold Plug N Plate Kit, but doing them one at a time is not really efficient.

Is it possible to make some sort of metal grid that the nuts can be screwed onto and then dipped in the solution all at once. If so ,how can I be sure the current is even throughout and that the voltage is correct, and also how long should it be immersed?

Any advice would be greatly appreciated.