View Single Post
  #2 (permalink)  
Old 11-14-2007, 07:58 PM
ed_denu ed_denu is offline
Experienced Metal Finisher
 
Join Date: Jul 2006
Posts: 279
ed_denu is on a distinguished road
Default Re: need help on elec. hardware

PID Temperature Controller
SSR(s) or Contactor(s) - one or more depending on load
Heat sink(s)
Element(s)
Hi temp wire running to elements
Electrical box to house components
THHN wire - appropriate gauge for amp load
Conduit and fittings
Hi-temp Fan
Electrical toggle switches for pid, fan, light
Porcelain light fixture and bulb
Service cord - appropriate size based on amp load
Receptacle, plug and boxes