Hey. May sound wierd, but plain white flour can bring back the shine. I always tell guys to never touch their freshly polished aluminum with a cleaning brush at the carwash. only water, maybe soap but no scrubbing. Aluminum always dulls in time, but the flour trick works well. Alot of truckers carry a bag of plain white flour to help their tanks/wheels look good. I was amazed, but it works pretty good.
Yeah, flour should work like talc.

I recommend my clients use good-quality microfiber cloths for washing.