View Single Post
  #6 (permalink)  
Old 11-16-2007, 09:24 PM
WolfeMacleod WolfeMacleod is offline
Newbie
 
Join Date: Nov 2007
Posts: 12
WolfeMacleod is on a distinguished road
Default Re: Anode + tank bar question

Quote:
Originally Posted by MrPontiac View Post
Wolfe, thought id drop you a note to say, i learned the hard way, do not leave your anodes in the solution will not in use, won,t last very long and at 40.00$ a pot well its not cheap either. I take mine out each time, wash em off with hot water, air dry.
Yeah, I was curious about that last night and did some searcing. Although I left them in last night, I think I'll take them out tonight and for the future.
I got two "OK" platings on a couple small brass peices last night. Not great, but OK. I wasn't using the agitator though, because there's not much room left once it's put in the bucket. I'm trying another one now, with the agitator, to see how well it works.

So, the anodes themselves...are they just plain nickel sheets?
Reply With Quote