I have a question about a part I did today. I sprayed Chevy Orange on a test strip of Aluminum and baked for 10 minutes at 400 degrees. I preheated the oven (an old kitchen oven) to 400 but when the timer went off I removed the strip and it had a dark look on it almost looked like it had started to burn. The powder instrucions said 375 for 25 minutes but being the hard head I am I did it my way. If I had left it at 375 for 25 minutes I am afraid it would have been too long. Any thoughts on this one? Thanks for the help guys.


How did you check the oven tenp?