Default Re: Deep Red came out Fuschia

Same here... my deep red comes out very red.
You didn't say what thickness you went for. Be sure to ano to a full 1 mil.
Does your mixed dye look dark red (it should). There is a remote possiblity you were given pink instead of red.
The other possibility is that your PH is off, or your mix is too week. Did you get every trace of dye out of the bottle when mixing?
Usually when the dye barely works, it's an indication of a lost connection. Any possiblity of that? If you used aluminum wire, check to see if the wires dyed, but the parts didn't.