NO!

I just looked up ONE SHOT and it contains solvents that act as an odour blanket and are also used to to disolve styrene products stuck down your drain.

Plating is a precise process that requires precise chemicals. Any additional chemical agents will cuase unexpected results.

As Jim said try any Auto store that sells lead acid Batteries. Look up batteries in your local Yelow pages or business listings and make a few calls.