Question What is the best way sand aluminum and to be able to do it fast?

I need some advice on how to sand aluminum really fast before polishing it because I do a lot of parts and need to do them quick . The way I’m doing it right now is I usually spray some VHT fast strip on it(On parts were VHT doesn’t work like on calipers I sandblast them) then I go over with greaseless compound on a spiral sewn with grits 240 and then 400. Once I’m done with that I polish with a sisal wheel that has black compound on it, and then a denim with white compound. The polisher I have now is a ¾ hp, 3600 rpm that is for 8 In wheels. So if anyone has better ways of polishing please let me know.
Thanks