Thread
:
my homemade powdercoating shop
View Single Post
#
6
(
permalink
)
11-25-2007, 05:11 PM
palmbeach
Amateur Metal Finisher
Join Date: Apr 2006
Posts: 60
Re: my homemade powdercoating shop
powder coating gun. 1 itw gema easyselect and 1 caswell 50 kv system. even though I have a pro gun I still use the caswell gun all the time for the smaller jobs
Attached Thumbnails
palmbeach
View Public Profile
Send a private message to palmbeach