Thanks 48 Buick. I think you're right on the cleaning issue. I had another plating session today and I had much better success. I super cleaned the parts and so far, no peeling. I also started rotating the part while in the chrome bath. Every once in awhile during the two minute plate, I would jiggle the part as well. They came out great! Did this with three additional items and all items came out with everything properly chrome plated. I think I'm beginning to get the hang of it now! Thanks for everyone's help on this forum for all the past questions I had. I'm sure there will be other questions later and its nice to now there are others out there willing to share their expertise.