Default Re: Powder Spray Booth for Dummies?...Need some help

our first simple booth was a walk-in that was 8'Lx4'Wx7'H. it was a pvc frame (maybe 2" or 2.5"?) with an mdf floor. the walls and ceiling were 6mil painter's tarp. we used 1/16" steel cable to cross brace the frame, hang parts from, and aid in grounding. later we added an mdf blower box with some house furnace filters. total cost on booth with an overhead light was well under $100, and the blower box with a 1200cfm squirrel cage blower was maybe $130. i'll post some pics.
__________________
Len
Figure Engineering, LLC