Re: copy chrome and rectifiers
With the three gallon kit you will be limited to the size piece you can fit into the tank
all of the old car emblems and ornaments were made from pot metal and I can say from experience this is a tough quest for a beginner and requires lots of practice
for this set up you will need Flash copper and copy chrome I would recommend at least a 10amp rectifier
__________________
Jim Eaton
|