Re: Ceramic Coating How To?
epoxy and polyester are very strong but epoxy is not UV stable
for polishing ceramic on a tumbler you need 1mm microbright ceramic balls and and acidic soap , you drop the part in for 10 minutes and it comers out highly polished.
|