My oven has two fans that I can vary the speed on from approx 200cfm to 800cfm each depending on the rpm I set it to. I found the correct size and shape elements for my oven in a NU-VU bakery oven then took the make model and serial number and ordered replacement parts.They are very similar to a household oven element just higher wattage and longer length.
|