sealant
im having trouble with the sealant i just bought, the colors after the ano are great, but after sealed the piece has white spots, and looses a bit of the color. yesterday y dyed two pieces that have the same dimensions and i did the same process on both, but i left one unsealed, and today the one unsealed has the same color than yesterday but the one sealed look like i said before, any ideas what is wrong??(im using the caswell's sealant the one that uses 1oz per gal)
|