The Gold S is a very nice gold.
Polish to a brilliant shine, then ano to only .5mil. Then dye for a relatively short period of time (2 to 5 minutes?). To me, a lighter color looks more like real gold.
__________________
Specializing in anodized graphics in Paintball guns.
|