You probably mean tripoli. It usually goes: emery (black), tripoli (brown). then white rouge. I usually skip the tripoli.
i usually get decent results with the denim spiral sewn wheels and the tripoli only. if the 7/8 arbor wheels won't fit onto your 1", maybe drill it out to an inch? shouldn't be a problem.