Quote:
Originally Posted by FigureLLC
our first simple booth was a walk-in that was 8'Lx4'Wx7'H. it was a pvc frame (maybe 2" or 2.5"?) with an mdf floor. the walls and ceiling were 6mil painter's tarp. we used 1/16" steel cable to cross brace the frame, hang parts from, and aid in grounding. later we added an mdf blower box with some house furnace filters. total cost on booth with an overhead light was well under $100, and the blower box with a 1200cfm squirrel cage blower was maybe $130. i'll post some pics.
|
Thanks a lot for the info. My main concern at this point is how to setup the filters and where to buy and what to look for as far as a fan/blower. Thats the part I have no clue what the ideal way to set that up is. I have access to have a nice frame for a booth made by a buddy of mine that does fabricating. I just need some info on the whole filtration situation.
Thanks again!