Default Re: Gun Finishing ???

Name the types of guns, and we can help you.

Usually on military-style rifles, you'll find most (if not all) surfaces are parkerized. Older styles could've been blued...

Usually the "silver" on handguns will be Nickel, though I've seen bonified Chrome-plated as well.