sealer tank needs to be stainless steel or plastic(polypropylene), and made up of D.I. water. If you use S.S. make sure you insulate the load bar if its metal so you don't have any stray currents that will cause pitting or white spots if there are chlorides present.
white spots are mainly caused by impurities in the water.
|