Quote:
Originally Posted by JAP_NDN View Post
The BMW valve cover looks good. How did you do all the sanding around the BMW lettering without rounding the edges of the letters (what tools did you use)? And how did you sand so closely to the letters in the recessed portions around them? Just curious 'cause I have to do the same thing. Mine looks about like yours did, too. Last thing: how long did it take? Thanks a bunch.
Yeah, anyway...actually when you need to get a piece done and move on to the next one, so far I've been successful in suggesting to my clients that the logo areas would look great painted, and I do it for them for free. Now if I had to do such an item for myself, the lettering would get done.

I use a homebuilt belt sander for such items, although it looks like I couldn't use it much on this particular cover. Would work great on the tops of the ribs etc. though.