Re: acid bath acting weird
One thing I forgot to mention is that to connect the wires to my cathodes I actually soldered the copper wire onto the lead, as in with a soldering iron . It seemed like a good idea at first, but I'm not so sure now.
I think I'll desolder those wires and replace them with something else, what do you recommend? I was thinking some heavy duty alligator clips.
|