You can get cheap bench top glass bead cabinets at Harbor-Freight. You need an air compressor to drive it, though. I know the price adds up. A wire wheel on a bench grinder might be a decent intermediate step if you're not ready to step up to a lot of other equipment. But for the record, my glass bead cabinet is the single greatest tool I've ever owned. I use it for everything--it's extremely useful. And glass bead cabinets don't make a mess since everything is contained inside the cabinet. I use mine in the house and it doesn't make a mess.[/url]