Rubbing a powder coated part with MEK or a xylene-MEK mixture is a way to test for a fully cured coating. Since acetone has properties similiar to MEK, a fully-cured powder coating (from any manufacturer's powder should be resistant to xylene and acetone.

However, I am not sure the coating would hold up to being soaked for extended periods in those chemicals.