Here's the latest from my sculpture studio. They are about four feet long. Mostly 22 and 24 ga. 304 stainless and 22 ga. cold rolled steel, with a little bar stock thrown in.





The most difficult part was beating those heels out of sheet metal. Stainless work hardens almost instantly. I hate the damn stuff, but I can't resist it; it's so gorgeous when you're finally done.